Automatic Melting Furnace Kg. 3
Electric Melting Furnace Kg. 3 - 1150° C
Electric Melting Furnace Kg. 3 - 1150° C
Red Silicone Rubber in sheet of 900 g.
Vulcanizing temperature: 170 - 180 °C.
Vulcanizing time: 1 hour.
Hardness: Shore 40.
Sheet size: mm 300 x 300 x 6.
Graphite Crucible for Induction Melting Machines CEIA F1
Freeman Flakes Injection Wax - Carvable Purple
Pack of 454 g.
Injection Temperature: 76-79ºC / 170-175ºF.
Superior carvability.
Boric acid powder for fusion
Bottle 1 kg.
Hazelnut Silicone Rubber Low Shrinkage in sheet of 900 g.
Vulcanizing temperature: 85 - 90 °C.
Vulcanizing time: 1 hour.
Hardness: Shore 44 - 46.
Shrinkage: 0,3 %.
Sheet size: mm 300 x 300 x 6.
Copper in sticks
Squared ceramic crucible cm 7x7
Freeman Flakes Injection Wax - Tuf Guy Green
Pack of 454 g.
Injection Temperature: 76ºC / 170ºF.
High toughness.
Fusimod Blue Silicone Rubber Low Shrinkage
Vulcanizing recommended temperature: 80 - 100 °C.
Vulcanizing time: 2 Minutes x mm.
Hardness: Shore 46.
Elongation (%): 610.
Tensile strenght (N/mm2): 8,9.
Tear strenght (N/mm): 17,4.
Shrinkage: minimum.
Sold in sheet of 500 g.
Sheet size: mm 330 x 180 x 6.
Freeman Flakes Injection Wax - Flexible Blue
Injection Temperature: 76º C / 170º F.
Pack of 454 g.
Highest Flexibility.
Surgical Scalpel Blade No.11
Graphite Crucible for 1 kg Melting Furnace
Graphite Crucible for 0,5 kg Melting Furnace
Pink Silicone Rubber in sheet of 900 g.
Vulcanizing temperature: 170 - 180 °C.
Vulcanizing time: 1 hour.
Hardness: Shore 44 - 46.
Shrinkage: 2,5 %.
Sheet size: mm 300 x 300 x 6.
Cast iron ingot mold g. 2600
Blue Silicone Rubber in sheet of 900 g.
Vulcanizing temperature: 170 - 180 °C.
Vulcanizing time: 1 hour.
Hardness: Shore 44 - 46.
Shrinkage: 2,5 %.
Sheet size: mm 300 x 300 x 6.
Wax Injector 145°C - 1.5 kg
Graphite Crucible for gas Furnace
Graphite Crucible for 2 kg Melting Furnace
White Alloy EM
Nickel Safe white Alloy Pandora ROLLY
High performance standard alloy for 18 carats, for mechanical works.
Color: white - standard color coordinates: L * = 85.5 a * = 2.8 b * = 14.5.
Nickel release UNI EN 1811: 2011: 0.14 μg / cm2 / week.
Zinc in drops
Sale by weight.
Unit of measure: Grams.
Electric Melting Furnace Kg. 2 - 1150° C
Crucible and Tongs included.
Mold Frames
Replacement manual pump for wax injectors
1/4" male thread.
Made in Italy.
Rubber Sprue bases for casting Flasks
Tree Style.
To purchase please select desided size.
Yellow Silicone Rubber in sheet of 900 g.
Vulcanizing temperature: 170 - 180 °C.
Vulcanizing time: 1 hour.
Hardness: Shore 50.
Shrinkage: 2,5 %.
Sheet size: mm 300 x 300 x 6.
Freeman Flakes Injection Wax - Filigree Pink
Pack of 454 g.
Injection Temperature: 73º C / 165º F.
Very high detail.
R&R ULTRA-VEST investment
Black smith's tongs
In forged steel, enamelled.
Type with flat straight noses.
Lenght mm 400.
Made in Italy.
Brass in drops
Colour: yellow.
This alloy can be used only for lost-wax casting.
To purchase please select desired package.
See-Thru Mold Frame
Contains 2 glass cover plates with 2 metal clamps and one center frame with a sprue former for making the sprue for the model.
Size: mm 53 x 50 x 90 h.
Made in USA.
R&R AURUM investment
Yellow Alloy for gold 2P18 Pandora
Cast iron Ingot Mold for wire
This mold can make six sizes of wire.
Made in Italy.
Ingot Size | Gold capacity |
mm 5 x 6 x 140 | g. 73 |
mm 8 x 6 x 140 | g. 118 |
mm 12 x 6 x 100 | g. 126 |
mm 6 x 6 x 140 | g. 88 |
mm 10 x 6 x 14 | g. 147 |
mm 20 x 6 x 100 | g. 210 |