Bronze in drops 90-10

Bronze in drops 90-10

Composition: Copper 90% - Tin 10%.

€38.05
Tax included
 In Stock

Description

Bronze in drops 90-10

Composition: Copper 90% - Tin 10%.

To purchase please select desired package.

This alloy can be used only for lost-wax casting.

Colour: yellow.

INDICATIONS FOR USE

Melting temperature: 980° C.

Casting temperatures:

  • 100° C above the melt temperature for casting with centrifugal machines.
  • 140° C above the melt temperature for casting in cylinders with intake.
  • 120° C above the melt temperature for casting in vacuum machines in controlled atmosphere.

 

Cylinders temperature: from 550° C to 650° C depending on the machine and the object size.

Cast items cooling: in water after 10 minutes.

Annealing: 620 ° C for 20 minutes followed by rapid cooling in hot water (min. 40 ° C).